■ Overview
RINA Grade AH36,RINA AH36,RINA AH36 steel plate is mainly used to building ships and vessels,so we also call this steel plate as RINA Grade AH36 ship plate,RINA Grade AH36 shipbuilding steel plate,RINA Grade AH36 marine steel plate or RINA Grade AH36 shipbuilding plate.Shipyards use shipbuilding steel plate RINA Grade AH36 to construct tanks and vessels in ships cause RINA Grade AH36 ship plate owned the higher yield strength and tensile strength.
■ Full Data
Technical Requirements & Additional Services for RINA AH36 steel plate:
♦ High tension test
♦ Z-Test (Z15,Z25,Z35)
♦ Low temperature impacting test
♦ Ultrasonic test under ASTM A435,A577,A578
♦ Cetificated by ABS,LR,GL,BV,DNV,KR,NK,CCS,RINA
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
♦ High tension test
♦ Z-Test (Z15,Z25,Z35)
♦ Low temperature impacting test
♦ Ultrasonic test under ASTM A435,A577,A578
♦ Cetificated by ABS,LR,GL,BV,DNV,KR,NK,CCS,RINA
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
■ Techicals
►Mechnical property for RINA Grade AH36 shipbuilding structual steel:
Yield strength (≥Mpa) | Tensile strength (Mpa) | Elongation in ≥,% | |
355 | 490-620 | 200mm | 50mm |
19 | 22 |
►Chemical composition for RINA Grade AH36 ship steel (Heat Analysis Max%)
Main chemical elements composition of RINA Grade AH36 | ||||||
C | Si | Mn | P | S | Al (acid) min. | Nb |
0.18 | 0.10-0.50 | 0.90-1.60 | 0.035 | 0.035 | 0.015 | 0.02-0.05 |
V | Ti | Cu | Cr | Ni | Mo | |
0.05-0.10 | 0.02 | 0.35 | 0.20 | 0.40 | 0.08 |