♦ Normalized Heat treatment at Temp.1020-1080 Deg.C and Tempered treatment at 730-780 Deg.C
♦ Flattening test according to EN 10233
♦ Ring Tensile test comply to EN 10237
♦ Impacting test comply to EN 10045-1
♦ Issued Orginal Mill test certificate under EN10204 3.1/3.2 FORMAT
♦ Surface Protection:Black,Varnish,Hot Dip Galvanized,Coating with shop prime
►Mechnical property for X20CrMoV11-1 seamless steel pipes:
X20CrMoV11-1 |
||||
Yield strength (≥Mpa) |
T≤16 |
16<T≤40 |
40<T≤60 |
60<T≤100 |
490 |
490 |
490 |
490 |
|
Tensile strength (≥Mpa) |
690-840 |
►Chemical composition for X20CrMoV11-1 Boiler steel pipes (Heat Analysis Max%)
Main chemical elements composition of X20CrMoV11-1 |
|||||
C |
Si |
Mn |
P |
S |
Cr |
0.17-0.23 |
0.15-0.50 |
1.00 |
0.025 |
0.020 |
10.0-12.5 |
Mo |
Ni |
Alt |
Cu |
V |
|
0.8-1.2 |
0.3-0.8 |
0.04 |
0.30 |
0.25-0.35 |
|