♦ Normalized Heat treatment at Temp.900-960 Deg.C and Tempered treatment at 680-750 Deg.C
♦ Flattening test according to EN 10233
♦ Ring Tensile test comply to EN 10237
♦ Impacting test comply to EN 10045-1
♦ Issued Orginal Mill test certificate under EN10204 3.1/3.2 FORMAT
♦ Surface Protection:Black,Varnish,Hot Dip Galvanized,Coating with shop prime
►Mechnical property for 10CrMo9-10 boiler steel pipes:
10CrMo9-10 |
||||
Yield strength (≥Mpa) |
T≤16 |
16<T≤40 |
40<T≤60 |
60<T≤100 |
280 |
280 |
270 |
- |
|
Tensile strength (≥Mpa) |
480-630 |
►Chemical composition for 10CrMo9-10 Boiler steel pipes (Heat Analysis Max%)
Main chemical elements composition of 10CrMo9-10 |
||||
C |
Si |
Mn |
P |
S |
0.08-0.14 |
0.50 |
0.30-0.70 |
0.025 |
0.020 |
Cr |
Mo |
Ni |
Alt |
Cu |
2.0-2.5 |
0.9-1.1 |
0.30 |
0.04 |
0.30 |