♦ Low temperature impacting test according to EN10045-1
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Surface Protection:Black,Varnish,Hot Dip Galvanized,Coating with shop prime
♦ Tolerances,dimensions and sectional properties according to to EN10210-2 Part 2
♦ Non destructive testing for steel tubes comply to EN 10246-3,EN10246-5,EN10246-8
►Mechnical property for S275J0H Steel Pipe:
Thickness (mm) |
||||||
|
≤ 16 |
> 16 ≤ 40 |
> 40 ≤ 63 |
> 63 ≤ 80 |
> 80 ≤ 100 |
> 100 ≤ 120 |
Yield strength (≥Mpa) |
275 |
265 |
255 |
245 |
235 |
225 |
|
< 3 |
≥ 3 ≤ 100 |
> 100 ≤ 120 |
|||
Tensile strength (Mpa) |
430-580 |
410-560 |
400-540 |
►Chemical composition for S275J0H Steel pipe (Ladle Analysis Max%)
Main chemical elements composition of S275J0H |
||||||
Thickness(mm) |
C |
Si |
Mn |
P |
S |
N |
T≤40 |
0.20 |
... |
1.50 |
0.035 |
0.035 |
0.009 |
40<T≤120 |
0.22 |