■ Overview
For steel angles S355K2,the impacting test temperature shall be the same as steel plate S355J2 angle bars (both minus 20 centigree),however,S355K2 steel angles need a higher average impacting energy when doing test.Many stocks of high tension strength in Xinsteel with grades as S355JR angles,S355J0 steel angles,S355J2 angle bars,A572Gr50 angle steels,A573Gr58 L profiles.
■ Full Data
Technical Requirements & Additional Services:
♦ Low temperature impacting test
♦ Rolling under standard NACE MR-0175 (HIC+SSCC)
♦ Ultrasonic test under EN 10160,ASTM A435,A577,A578
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
♦ Low temperature impacting test
♦ Rolling under standard NACE MR-0175 (HIC+SSCC)
♦ Ultrasonic test under EN 10160,ASTM A435,A577,A578
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
■ Techicals
►Mechnical property for S355K2 low alloy steel angles:
Thickness (mm) | |||||||||
S355K2 | ≤ 16 | > 16 ≤ 40 | > 40 ≤ 63 | > 63 ≤ 80 | > 80 ≤ 100 | > 100 ≤ 150 | > 150 ≤ 200 | > 200 ≤ 250 | > 250 |
Yield strength (≥Mpa) | 355 | 345 | 335 | 325 | 315 | 295 | 285 | 275 | 265 |
< 3 | ≥ 3 ≤ 100 | > 100 ≤ 150 | > 150 ≤ 250 | > 250 | |||||
Tensile strength (Mpa) | 510-680 | 470-630 | 450-600 | 450-600 | 450-600 |
►Chemical composition for S355K2 low alloy steel angles (Ladle Analysis Max%)
Main chemical elements composition of S355K2 | |||||||
Thickness(mm) | C | Si | Mn | P | S | N | Cu |
T≤16 | 0.20 | 0.55 | 1.60 | 0.025 | 0.025 | ... | 0.55 |
16<T≤40 | 0.20 | ||||||
40<T | 0.22 |