♦ Heat treatment Normalize and Temper,Austenitizing / Solutioning Temperature range 1040-1080 Degree.C.
♦ General requirements for these tubes in A213/A213M shall be comply to A1016/A1016M
♦ Mill test certificate with EN 10204 TYPE 3.1 OR 3.2
♦ Surface Protection:Black,Varnish,Hot Dip Galvanized,Coating with shop prime
►Mechnical property for A213 Grade T91 seamless steel tube:
A213 Gr T91 steel pipe | |
Yield strength (≥Mpa) |
415 |
Tensile strength (≥Mpa) |
585 |
►Chemical composition for A213 Grade T91 seamless steel pipe (Heat Analysis Max%)
Main chemical elements composition of A213 Grade T91 |
|||||||
C |
Mn |
P |
S |
Si |
Ni |
Cr |
Mo |
0.08-0.12 |
0.30-0.60 |
0.020 |
0.010 |
0.25-0.50 |
0.40 |
8.0-9.5 |
0.85-1.05 |
V |
N | Al | Cb | Ti | Zr | ||
0.18-0.25 |
0.03-0.07 |
0.02 |
0.06-0.10 |
0.01 |
0.01 |