■ Overview
EN 10225 S420G1+M,S420G1+M steel plate,S420G1+M steel sheet is mainly used in steel structures.This steel standard specification S420 includes four different steel grades S420G1+QT,S420G1+M,S420G2+QT and S420G2+M.They have owned different chemical composition and mechanical property.Oil and offshore platform steel plate S420G1+M owned the minimum yield strength at 420Mpa,and the tensile strength shall be above 500 Mpa.TMCP heat treatment is necessary for steel plate S420G1+M for any thickness when rolling.
■ Full Data
Technical Requirements & Additional Services for S420G1+M steel plate:
♦ Z TEST (Z15,Z25,Z35)
♦ Low temperature impacting test
♦ Ultrasonic test under EN 10160,ASTM A435,A577,A578
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
♦ Z TEST (Z15,Z25,Z35)
♦ Low temperature impacting test
♦ Ultrasonic test under EN 10160,ASTM A435,A577,A578
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
■ Techicals
►Mechnical property for S420G1+M steel plate:
Thickness (mm) | |||||
S420G1+M | ≤ 16 | > 16 ≤ 40 | > 40 ≤ 63 | > 63 ≤ 80 | > 80 |
Yield strength (≥Mpa) | 420 | 400 | 390 | 380 | 380 |
≤ 40 | > 40 | ||||
Tensile strength (Mpa) | 500 | 480 |
►Chemical composition for S420G1+M steel plate (Ladle Analysis Max%)
Main chemical elements composition of S420G1+M steel plate | ||||||||
C | Si | Mn | P | S | Cr | Mo | Nb+V | Nb+V+Ti |
0.14 | 0.15-0.55 | 1.65 | 0.020 | 0.010 | 0.25 | 0.25 | 0.09 | 0.11 |
Ni | Alt | Cu | N | Nb | Ti | V | Cr+Mo+Ni+Cu | |
0.70 | 0.015-0.055 | 0.30 | 0.010 | 0.040 | 0.025 | 0.080 | 0.90 |