Quenched and tempered treated 10CrMo9-10,10CrMo9-10 steel plate,10CrMo9-10 steel sheet owned high steel properties.For steel plate thicknesses greater than 150 mm, a maximum content of 0,17% C may be agreed upon at the time of enquiry and order.Types of inspection and inspection documents for steel 10CrMo9-10 according to EN 10028-1.
♦ High tension test
♦ Low temperature impacting test
♦ Simulated post-welded heat treatment (PWHT)
♦ Ultrasonic test under EN 10160,ASTM A435,A577,A578
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
►Mechnical property for 10CrMo9-10 steel plate:
Thickness(mm) | Yield strength (≥Mpa) | Tensile strength (Mpa) | Elongation in ≥,% |
T≤16 | 310 | 480-630 | 18 |
16<T≤40 | 300 | ||
40<T≤60 | 290 | ||
60<T≤100 | 280 | 470-620 | 17 |
100<T≤150 | 260 | 460-610 | |
150<T | 250 | 450-600 |
►Chemical composition for 10CrMo9-10 steel plate (Heat Analysis Max%)
Main chemical elements composition of 10CrMo9-10 steel plate | ||||||||
C | Si | Mn | P | S | N | Cr | Cu | Mo |
0.08-0.14 | 0.50 | 0.40-0.80 | 0.020 | 0.010 | 0.012 | 2.00-2.50 | 030 | 0.90-1.10 |