■ Overview
DNV Grade FH36,NV F36,DNV FH36 steel plate,also named as DNV Grade FH36 marine steel plate which have to be done low temperature impacting test under minus 60 centigree and done normalized or TMCP heat treatment for any thickness.Else,our engineers suggest our end users to choose Z-test for ship steel plate DNV Grade FH36 to improved the strength in thickness direction,they can choose three different classes for Z-Test,Z15,Z25 and Z35.
■ Full Data
Technical Requirements & Additional Services for DNV FH36 steel plate:
♦ High tension test
♦ Z-Test (Z15,Z25,Z35)
♦ Low temperature impacting test
♦ Ultrasonic test under ASTM A435,A577,A578
♦ Cetificated by ABS,LR,GL,BV,DNV,KR,NK,CCS,RINA
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
♦ High tension test
♦ Z-Test (Z15,Z25,Z35)
♦ Low temperature impacting test
♦ Ultrasonic test under ASTM A435,A577,A578
♦ Cetificated by ABS,LR,GL,BV,DNV,KR,NK,CCS,RINA
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
■ Techicals
►Mechnical property for DNV Grade FH36 shipbuilding plate:
Yield strength (≥Mpa) | Tensile strength (Mpa) | Elongation in ≥,% | |
355 | 490-620 | 200mm | 50mm |
19 | 22 |
►Chemical composition for DNV Grade FH36 ship plate (Heat Analysis Max%)
Main chemical elements composition of DNV Grade FH36 | ||||||
C | Si | Mn | P | S | Al (acid) min. | Nb |
0.16 | 0.50 | 0.90-1.60 | 0.025 | 0.025 | 0.015 | 0.02-0.05 |
V | Ti | Cu | Cr | Ni | Mo | N |
0.03-0.10 | 0.02 | 0.35 | 0.20 | 0.80 | 0.08 | 0.009 |