■ Overview
With alloy elements especially the element Nickel,ABS Grade FH36,ABS FH36 steel plate,ABS FH36 ship plate can bear the weather corrosion when using to build ships and vessels.When rolling ABS Grade FH36 steel plate,the steel should be chosed as full killed and hot rolling.Normalized heat treatment have to be done when the steel billets finished.Low temperature impacting test should be made under minus 60 centigrade.
■ Full Data
Technical Requirements & Additional Services for ABS FH36 ship plate:
♦ High tension test
♦ Z-Test (Z15,Z25,Z35)
♦ Low temperature impacting test
♦ Ultrasonic test under ASTM A435,A577,A578
♦ Cetificated by ABS,LR,GL,BV,DNV,KR,NK,CCS,RINA
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
♦ High tension test
♦ Z-Test (Z15,Z25,Z35)
♦ Low temperature impacting test
♦ Ultrasonic test under ASTM A435,A577,A578
♦ Cetificated by ABS,LR,GL,BV,DNV,KR,NK,CCS,RINA
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
■ Techicals
►Mechnical property for ABS Grade FH36 shipbuilding plate:
Yield strength (≥Mpa) | Tensile strength (Mpa) | Elongation in ≥,% | |
355 | 490-620 | 200mm | 50mm |
19 | 22 |
►Chemical composition for ABS Grade FH36 ship plate (Heat Analysis Max%)
Main chemical elements composition of ABS Grade FH36 | ||||||
C | Si | Mn | P | S | Al (acid) min. | Nb |
0.16 | 0.50 | 0.90-1.60 | 0.025 | 0.025 | 0.015 | 0.02-0.05 |
V | Ti | Cu | Cr | Ni | Mo | N |
0.03-0.10 | 0.02 | 0.35 | 0.20 | 0.80 | 0.08 | 0.009 |