■ Overview
RINA Grade FH36,RINA FH36,RINA FH36 steel plate,also named as RINA Grade FH36 marine steel plate which have to be done low temperature impacting test under minus 60 centigree and done normalized heat treatment for any thickness.Else,our engineers suggest our end users to choose Z-test for ship steel plate RINA Grade FH36 to improved the strength in thickness direction,they can choose three different classes for Z-Test,Z15,Z25 and Z35.
■ Full Data
Technical Requirements & Additional Services for RINA FH36 steel plate:
♦ High tension test
♦ Z-Test (Z15,Z25,Z35)
♦ Low temperature impacting test
♦ Ultrasonic test under ASTM A435,A577,A578
♦ Cetificated by ABS,LR,GL,BV,DNV,KR,NK,CCS,RINA
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
♦ High tension test
♦ Z-Test (Z15,Z25,Z35)
♦ Low temperature impacting test
♦ Ultrasonic test under ASTM A435,A577,A578
♦ Cetificated by ABS,LR,GL,BV,DNV,KR,NK,CCS,RINA
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
■ Techicals
►Mechnical property for RINA Grade FH36 shipbuilding structual steel:
Yield strength (≥Mpa) | Tensile strength (Mpa) | Elongation in ≥,% | |
355 | 490-620 | 200mm | 50mm |
19 | 22 |
►Chemical composition for RINA Grade FH36 ship steel (Heat Analysis Max%)
Main chemical elements composition of RINA Grade FH36 | ||||||
C | Si | Mn | P | S | Al (acid) min. | Nb |
0.16 | 0.50 | 0.90-1.60 | 0.025 | 0.025 | 0.015 | 0.02-0.05 |
V | Ti | Cu | Cr | Ni | Mo | N |
0.03-0.10 | 0.02 | 0.35 | 0.20 | 0.80 | 0.08 | 0.009 |