♦ Low temperature impacting test at Minus 40 Deg.C.
♦ Cutting and welding as per end user’s demands.
♦ More restriction for Chromium and Cooper elements contains.
♦ Ultrasonic test under EN 10160,ASTM A435,A577,A578.
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Packing with pallets,wooden cases,bundled with iron belts.
►Mechnical property for TB/T 1979 Q350EWR1 STEEL PLATE
Mechanical Property for Q350EWR1 steel plate |
||
Yield strength (≥Mpa) |
Tensile strength (Mpa) |
Elongation % ≥ |
350 |
490-690 |
22 |
►Chemical composition for TB/T 1979 Q350EWR1 STEEL PLATE (Heat Analysis Max%)
Main chemical elements composition of Q350EWR1 |
|||||||
C |
Si |
Mn |
P |
S |
Cu |
Cr |
Ni |
0.07 |
0.50 |
1.10 |
0.020 |
0.010 |
0.30-0.55 |
3.0-5.5 |
0.1-0.65 |