♦ Normalized at Temp.1040-1080 Deg.C and Tempered Heat treatment at Temp.750-780 Deg.C
♦ Flattening test according to GB/T 246
♦ Bending test comply to GB/T 232
♦ Microstructure examination comply to GB/T 13298
♦ Issued Orginal Mill test certificate under 3.1/3.2 FORMAT
♦ Surface Protection:Black,Varnish,Hot Dip Galvanized,Coating with shop prime
►Mechnical property for 07Cr2MoW2VNbB boiler steel pipes:
07Cr2MoW2VNbB |
|
Yield strength (≥Mpa) |
400 |
Tensile strength (≥Mpa) |
510 |
►Chemical composition for 07Cr2MoW2VNbB boiler steel pipes (Heat Analysis Max%)
Main chemical elements composition of 07Cr2MoW2VNbB |
|||||||
C |
Si |
Mn |
P |
S |
Cr |
W |
Alt |
0.04-0.10 |
0.50 |
0.10-0.60 |
0.025 |
0.010 |
1.90-2.60 |
1.45-1.75 |
0.03 |
Cu |
Ni |
Mo |
V |
Ti |
B |
Nb |
N |
0.20 |
0.30 |
0.05-0.30 |
0.20-0.30 |
0.08-0.18 |
0.005-0.006 |
0.02-0.08 |
0.03 |