♦ Low temperature impact test at -40 ℃ with minimum energy at 27J on transverse direction
♦ Minimum yield strength for P355NL1 seamless tube above 355 Mpa
♦ Ring Tensile test comply to EN 10237
♦ An inspection certificate 3.1.B issued in according with EN 10204 generally
♦ Surface Protection:Black,Varnish,Hot Dip Galvanized,Coating with shop prime
►Mechnical property for P355NL1 seamless pipe
P355NL1 seamless pipe |
|||||||
Thickness |
T≤12 |
12<T≤20 |
20<T≤40 |
40<T≤50 |
50<T≤65 |
65<T≤80 |
80<T |
Yield strength (≥Mpa) |
355 |
355 |
345 |
335 |
325 |
315 |
305 |
Tensile strength (≥Mpa) |
490 to 650 |
490 to 630 |
450 to 590 |
►Chemical composition for P355NL1 seamless pipe (Heat Analysis Max%)
Main chemical elements composition of P355NL1 |
|||||||
C |
Mn |
P |
S |
Si |
Cr |
Mo |
Ni |
0.18 |
0.9-1.7 |
0.025 |
0.020 |
0.50 |
0.3 |
0.08 |
0.50 |
Alt |
Cu |
N |
Nb |
Ti |
V |
Nb+Ti+V |
|
0.02 |
0.3 |
0.02 |
0.05 |
0.04 |
0.10 |
0.12 |