♦ Normalized Heat treatment at Temp.1040-1080 Deg.C and Tempered treatment at 740-780 Deg.C
♦ Flattening test according to EN 10233
♦ Ring Tensile test comply to EN 10237
♦ Impacting test comply to EN 10045-1
♦ Issued Orginal Mill test certificate under EN10204 3.1/3.2 FORMAT
♦ Surface Protection:Black,Varnish,Hot Dip Galvanized,Coating with shop prime
►Mechnical property for X11CrMoWVNb9-1-1 seamless steel pipes:
X11CrMoWVNb9-1-1 |
||||
Yield strength (≥Mpa) |
T≤16 |
16<T≤40 |
40<T≤60 |
60<T≤100 |
450 |
450 |
450 |
450 |
|
Tensile strength (≥Mpa) |
620-850 |
►Chemical composition for X11CrMoWVNb9-1-1 Boiler steel pipes (Heat Analysis Max%)
Main chemical elements composition of X11CrMoWVNb9-1-1 |
||||||
C |
Si |
Mn |
P |
S |
Cr |
Mo |
0.09-0.13 |
0.10-0.50 |
0.30-0.60 |
0.020 |
0.010 |
8.5-9.5 |
0.9-1.1 |
Ni |
Alt |
Nb |
V |
N |
B |
W |
0.10-0.40 |
0.04 |
0.06-0.10 |
0.18-0.25 |
0.05-0.09 |
0.0005-0.005 |
0.9-1.1 |