♦ Normalized Heat treatment at Temp.920-960 Deg.C
♦ Flattening test according to EN 10233
♦ Ring Tensile test comply to EN 10237
♦ Impacting test comply to EN 10045-1
♦ Issued Orginal Mill test certificate under EN10204 3.1/3.2 FORMAT
♦ Surface Protection:Black,Varnish,Hot Dip Galvanized,Coating with shop prime
►Mechnical property for 8MoB5-4 boiler steel pipes:
8MoB5-4 |
||||
Yield strength (≥Mpa) |
T≤16 |
16<T≤40 |
40<T≤60 |
60<T≤100 |
400 |
- |
- |
- |
|
Tensile strength (≥Mpa) |
540-690 |
►Chemical composition for 8MoB5-4 Boiler steel pipes (Heat Analysis Max%)
Main chemical elements composition of 8MoB5-4 |
|||||
C |
Si |
Mn |
P |
S |
Cr |
0.06-0.10 |
0.10-0.35 |
0.60-0.80 |
0.025 |
0.020 |
0.20 |
Mo |
Alt |
Cu |
Ti |
B |
|
0.40-0.50 |
0.06 |
0.30 |
0.06 |
0.002-0.006 |