♦ Normalized Heat treatment at Temp.900-960 Deg.C
♦ Flattening test according to EN 10233
♦ Ring Tensile test comply to EN 10237
♦ Impacting test comply to EN 10045-1
♦ Issued Orginal Mill test certificate under EN10204 3.1/3.2 FORMAT
♦ Surface Protection:Black,Varnish,Hot Dip Galvanized,Coating with shop prime
►Mechnical property for 20MnNb6 boiler steel pipes:
20MnNb6 |
||||
Yield strength (≥Mpa) |
T≤16 |
16<T≤40 |
40<T≤60 |
60<T≤100 |
355 |
345 |
335 |
- |
|
Tensile strength (≥Mpa) |
500-650 |
►Chemical composition fo 20MnNb6 Boiler steel pipes (Heat Analysis Max%)
Main chemical elements composition of 20MnNb6 |
|||||||
C |
Si |
Mn |
P |
S |
Alt |
Cu |
Nb |
0.22 |
0.15-0.35 |
1.0-1.5 |
0.025 |
0.020 |
0.060 |
0.30 |
0.015-0.10 |