♦ Quenched Heat treatment at Temp.980-1030 Deg.C and Tempered treatment at 680-730 Deg.C
♦ Flattening test according to EN 10233
♦ Ring Tensile test comply to EN 10237
♦ Impacting test comply to EN 10045-1
♦ Issued Orginal Mill test certificate under EN10204 3.1/3.2 FORMAT
♦ Surface Protection:Black,Varnish,Hot Dip Galvanized,Coating with shop prime
►Mechnical property for 20CrMoV13-5-5 boiler steel pipes:
20CrMoV13-5-5 |
||||
Yield strength (≥Mpa) |
T≤16 |
16<T≤40 |
40<T≤60 |
60<T≤100 |
590 |
590 |
590 |
- |
|
Tensile strength (≥Mpa) |
740-880 |
►Chemical composition for 20CrMoV13-5-5 Boiler steel pipes (Heat Analysis Max%)
Main chemical elements composition of 20CrMoV13-5-5 |
|||||
C |
Si |
Mn |
P |
S |
V |
0.17-0.23 |
0.15-0.35 |
0.30-0.50 |
0.025 |
0.020 |
0.45-0.55 |
Cr |
Mo |
Ni |
Alt |
Cu |
|
3.0-3.3 |
0.5-0.6 |
0.30 |
0.04 |
0.30 |
|