■ Overview
Low alloy steel angles S450J0 is a kind steel grade in European standard EN 10025-2.Angle steel bar S450J0 owned the minimum yield strength at 450 Mpa for high tension.S450J0 steel angles is a kind carbon structure steel which is used in riveted,bolted or welded construction of bridges and buildings,and for general structural purpose.
■ Full Data
Technical Requirements & Additional Services:
♦ Low temperature impacting test
♦ Rolling under standard NACE MR-0175 (HIC+SSCC)
♦ Ultrasonic test under EN 10160,ASTM A435,A577,A578
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
♦ Low temperature impacting test
♦ Rolling under standard NACE MR-0175 (HIC+SSCC)
♦ Ultrasonic test under EN 10160,ASTM A435,A577,A578
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
■ Techicals
►Mechnical property for S450J0 low alloy steel angles:
Thickness (mm) | |||||||||
S450J0 | ≤ 16 | > 16 ≤ 40 | > 40 ≤ 63 | > 63 ≤ 80 | > 80 ≤ 100 | > 100 ≤ 150 | > 150 ≤ 200 | > 200 ≤ 250 | > 250 |
Yield strength (≥Mpa) | 450 | 430 | 410 | 390 | 380 | 380 | 380 | 380 | 380 |
< 3 | ≥ 3 ≤ 100 | > 100 ≤ 150 | > 150 ≤ 250 | > 250 | |||||
Tensile strength (Mpa) | 550-720 | 530-700 | 530-700 | 530-700 | 530-700 |
►Chemical composition for S450J0 low alloy steel angles (Ladle Analysis Max%)
Main chemical elements composition of S450J0 | |||||||
Thickness(mm) | C | Si | Mn | P | S | N | Cu |
T≤16 | 0.20 | 0.55 | 1.70 | 0.030 | 0.030 | 0.025 | 0.55 |
16<T≤40 | 0.20 | ||||||
40<T | 0.22 |