■ Overview
DIN 17100 St44-2 steel angles is mainly delivered in hot rolled or normalized condition after production for general structural purposes in steel industry.Xinsteel conform to the chemical composition table as belows.It is permissible to exceed the maximum value indicated,provided a phosphorous content per 0.001% N of 0.005% P below the maximum value indicated is maintained.The Nitrogen content may not,however,exceed a value of 0.0012% N in the ladle analysis and 0.0014% N in the product analysis for steel plate St44-2.
■ Full Data
Technical Requirements & Additional Services:
♦ Low temperature impacting test
♦ Rolling under standard NACE MR-0175 (HIC+SSCC)
♦ Ultrasonic test under EN 10160,ASTM A435,A577,A578
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
♦ Low temperature impacting test
♦ Rolling under standard NACE MR-0175 (HIC+SSCC)
♦ Ultrasonic test under EN 10160,ASTM A435,A577,A578
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
■ Techicals
►Mechnical property for St44-2 Structural steel angles:
Thickness (mm) | |||||
St44-2 | ≤ 16 | > 16 ≤ 40 | > 40 ≤ 63 | > 63 ≤ 80 | > 80 |
Yield strength (≥Mpa) | 275 | 265 | 255 | 245 | 235 |
< 3 | ≥ 3 ≤ 100 | > 100 | |||
Tensile strength (Mpa) | 430-580 | 410-540 | 410-540 |
►Chemical composition for St44-2 Structural steel angles (Product Analysis Max%)
Main chemical elements composition of St44-2 | ||||||
Thickness(mm) | C | Si | Mn | P | S | N |
T≤40 | 0.24 | 0.60 | 1.70 | 0.060 | 0.060 | 0.010 |
T>40 | 0.25 |