■ Overview
The minimum yield strength of A283GrA steel tube is above 165Mpa and tensile strength is within 310-415 Mpa when offering.ASTM A283/A283M specification contains A283 Grade A steel pipe,A283 Grade B steel pipe,A283 Grade C steel pipe and A283 Grade D steel pipe.
■ Full Data
Technical Requirements & Additional Services for ASTM A283GrA steel pipe:
♦ Low temperature impacting test
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Surface Protection:Black,Varnish,Hot Dip Galvanized,Coating with shop prime
♦ Tolerances,dimensions and sectional properties according to to ASTM A6/A6M
♦ Non destructive testing for steel tubes comply to ASTM A435/A435M,A577/A577M,A578/A578M
♦ Low temperature impacting test
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Surface Protection:Black,Varnish,Hot Dip Galvanized,Coating with shop prime
♦ Tolerances,dimensions and sectional properties according to to ASTM A6/A6M
♦ Non destructive testing for steel tubes comply to ASTM A435/A435M,A577/A577M,A578/A578M
■ Techicals
►Mechnical property for A283 Grade A steel pipe:
►Chemical composition for A283 Grade A steel pipe (Heat Analysis Max%)
Yield strength (≥Mpa) | Tensile strength (Mpa) | Elongation in ≥,% | |
165 | 310-415 | 200mm | 50mm |
27 | 30 |
►Chemical composition for A283 Grade A steel pipe (Heat Analysis Max%)
Main chemical elements composition of A283 Grade A steel pipe | ||||||
Thickness(mm) | C | Si | Mn | P | S | Cu (Min.) Cooper steel |
T≤40 | 0.14 | 0.40 | 0.90 | 0.035 | 0.04 | 0.20 |
40<T | 0.15-0.40 |