♦ Heat treatment Normalize and Temper,Austenitizing / Solutioning Temperature range 1040-1080 Degree.C.
♦ General requirements for these tubes in A213/A213M shall be comply to A1016/A1016M
♦ Mill test certificate with EN 10204 TYPE 3.1 OR 3.2
♦ Surface Protection:Black,Varnish,Hot Dip Galvanized,Coating with shop prime
►Mechnical property for A213 Grade T911 steel pipe:
A213 T911 steel pipe | |
Yield strength (≥Mpa) |
440 |
Tensile strength (≥Mpa) |
620 |
►Chemical composition for A213 Grade T911 seamless steel pipe (Heat Analysis Max%)
Main chemical elements composition of A213 T911 |
|||||||
C |
Mn |
P |
S |
Si |
Ni |
Cr |
Mo |
0.09-0.13 |
0.30-0.60 |
0.020 |
0.010 |
0.10-0.50 |
0.40 |
8.5-9.5 |
0.9-1.1 |
V |
Cb | N | Al | W | B | Zr | Ti |
0.18-0.25 |
0.06-0.10 |
0.04-0.09 |
0.02 |
0.9-1.1 |
0.0003-0.006 | 0.01 | 0.01 |