♦ Normalising or Normalising Rolling heat treatment
♦ Cutting,Welding,Machining,Milling as per end user’s CAD drawing
♦ Shot blasting comply to SA 2.5 or SSPC and painting with shop primer
♦ More striction on some chemical elements contains for special applications
♦ Non-destructive inspection under GB/T2970,JB4730,EN 10160,ASTM A435,A577,A578
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2 with ABS,LR,BV,DNV-GL,SGS
►Mechnical property for GB/T 1591-2018 Q420NE STEEL PLATE
Mechanical Property for Q420NE steel plate |
||||||||
|
Thickness (mm) |
|||||||
Yield strength (≥Mpa) |
T≤16 |
16<T≤40 |
40<T≤63 |
63<T≤80 |
80<T≤100 |
100<T≤150 |
150<T≤200 |
200<T |
420 |
400 |
390 |
370 |
360 |
340 |
330 |
320 |
|
Tensile strength (Mpa) |
T≤100 |
100<T≤200 |
200<T |
|||||
520-680 |
500-650 |
500-650 |
►Chemical composition for GB/T 1591-2018 Q420NE STEEL PLATE (Heat Analysis Max%)
Main chemical elements composition of Q420NE |
||||||
C |
Si |
Mn |
P |
S |
Nb |
V |
0.20 |
0.60 |
1.00-1.70 |
0.025 |
0.020 |
0.01-0.05 |
0.01-0.20 |
Ti |
Cr |
Ni |
Cu |
Mo |
N |
Als Min. |
0.006-0.05 |
0.30 |
0.80 |
0.40 |
0.10 |
0.025 |
0.015 |