►Mechnical property for 07CR19NI10 stainless plate
07CR19NI10 stainless plate |
||||
Yield strength (≥Mpa) |
Tensile strength (≥Mpa) |
Elogation in 50mm min. % |
Hardness, Max |
|
Brinell HBW |
Rockwell HRBW |
|||
205 |
515 |
40 |
201 |
92 |
►Chemical composition for 07CR19NI10 stainless plate (Heat Analysis Max%)
Main chemical elements composition of 07CR19NI10 stainless plate |
|||||
C |
Mn |
P |
S |
Si |
Cr |
0.04-0.10 |
2.00 |
0.045 |
0.030 |
0.75 |
18.0-20.0 |
Ni |
N |
Cu |
Mo |
Al |
Ti |
8.0-10.5 |
- |
- |
- |
- |
- |