♦ Solution treatment or Annealing range is between 1850 and 2050F and cool rapidly
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Practices for detecting susceptibility to Intergranular corrosion in Austenitic stainless steels
♦ PMI test report,Cutting and welding as per end user’s demands
♦ Packing with water-resistance paper and Non-fumigation wooden crates
►Mechnical property for stainless steel plate 022cr17ni12mo2
stainless steel plate 022cr17ni12mo2 |
||||
Yield strength (≥Mpa) |
Tensile strength (≥Mpa) |
Elogation in 50mm min. % |
Hardness, Max |
|
Brinell HBW |
Rockwell HRBW |
|||
170 |
485 |
40 |
217 |
95 |
►Chemical composition for stainless steel plate 022cr17ni12mo2 (Heat Analysis Max%)
Main chemical elements composition of stainless steel plate 022cr17ni12mo2 |
|||||
C |
Mn |
P |
S |
Si |
Cr |
0.030 |
2.00 |
0.045 |
0.030 |
0.75 |
16.0-18.0 |
Ni |
Mo |
N |
Cb |
Al |
Ti |
10.0-14.0 |
2.0-3.0 |
0.10 |
- |
- |
- |