Comparasion of ABS FH36 plate and ABS EH36 steel plate
ABS FH36 steel plate and ABS EH36 steel plate are both high tensile strength steel materials for marine hull structural usage.Comparasion of ABS FH36 steel plate and ABS EH36 steel plate,what is the difference ? ABS FH36 plate need to be done -60℃ low temperature impacting test,but ABS EH36 plate done impacting test at -40℃.ABS FH36 steel plate and ABS EH36 steel plate shall be delivery as TMCP or Normalized.
Xinsteel Industrial keeps thousands tons shipbuilding steel plate stock with classification societies approval as ABS,LR,CCS,NK,DNV-GL,BV,KR.Steel grades as A,B,D,E,AH36,AH40,DH36,DH40,EH36,FH36.
ABS FH36 vs ABS EH36 |
Chemical composition: Heat Analysis Max% |
|||||||||
Standard |
Grade |
C |
Mn |
P |
S |
Si |
Cr |
Cu |
Nb |
V |
ABS |
FH36 |
0.16 |
0.9-1.6 |
0.025 |
0.025 |
0.5 |
0.20 |
0.35 |
0.02-0.05 |
0.03-0.10 |
ABS |
EH36 |
0.18 |
0.9-1.6 |
0.035 |
0.035 |
0.1-0.5 |
0.20 |
0.35 |
0.02-0.05 |
0.05-0.10 |
Mechanical Properties: |
Yield strength |
Tensile strength |
||||||||
Mpa Min. |
Mpa |
|||||||||
ABS |
FH36 |
355 |
490-620 |
|||||||
ABS |
EH36 |
355 |
490-620 |