A514 steel materials belongs to ASTM A514/A514M specification high yield strength,Quenched and tempered alloy steel plates which stuitable for welding,ASTM is the Acronym of American Society of Testing Materials.However,T-1 or T1 belongs to ArcelorMittal USA plate steels is a group of quenched and tempered constructional alloy steels with an attractive combination of advantages and characteristics.All steel grades in A514 and T-1 owned minimum yield strength above 690Mpa / 100 Ksi.As per chemical composition,A514 Grade F equivalent to T-1.T-1 type A is similar equivalent to A514 Grade B,T-1 type B is equivalent to A514 Grade H in chemical composition.
Heat treatment with Quenched and tempered,low temperature impacting test normally at -50 Deg.C and Ultrasonic examination comply to astm a435/a435m,a578/a578m shall be done for steel materials astm a514 grades and Arcelormittal T-1 steel materials typy.
High strength steel grades A514GrF vs T-1 |
Chemical composition: Heat Analysis Max% |
|||||||||||
Standard |
Grade |
C |
Mn |
P |
S |
Si |
Cr |
Ni |
Cu |
Mo |
V |
B |
U.S. |
T-1 |
0.1-0.2 |
0.6-1.0 |
0.035 |
0.04 |
0.15-0.35 |
0.4-0.65 |
0.7-1.0 |
0.15-0.5 |
0.4-0.6 |
0.03-0.08 |
0.0005-0.006 |
ASTM A514/A514M |
A514GrF |
0.1-0.2 |
0.6-1.0 |
0.035 |
0.04 |
0.15-0.35 |
0.4-0.65 |
0.7-1.0 |
0.15-0.5 |
0.4-0.6 |
0.03-0.08 |
0.0005-0.006 |
Mechanical Properties: |
Thickness |
Yield strength |
Tensile strength |
|||||||||
|
|
Mpa Min. |
Mpa |
|||||||||
U.S. |
T-1 |
T≤65 |
690 |
760-895 |
||||||||
ASTM A514/A514M |
A514 |
T≤65 |
690 |
760-895 |