■ Overview
Structural S460NL,S460NL steel plate,S460NL steel sheet is in steel standard EN 10025-3.Normalized heat treatment and Low temperature impacting test under -50 centigrade shall be done for steel plate S460NL.For hot rolled steel plate tolerances of steel S460NL the basic requirements shall be in accordance with EN 10029, including thickness tolerances to class A, unless otherwise agreed at the time of the order.Steel plate S460NL shall be suitable for welding,and general requirements for arc welding of the steel S460NL shall be given in EN 1011-2.
■ Full Data
Technical Requirements & Additional Services for S460NL steel plate:
♦ Low temperature impacting test
♦ Rolling under standard NACE MR-0175 (HIC+SSCC)
♦ Ultrasonic test under EN 10160,ASTM A435,A577,A578
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
♦ Low temperature impacting test
♦ Rolling under standard NACE MR-0175 (HIC+SSCC)
♦ Ultrasonic test under EN 10160,ASTM A435,A577,A578
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
■ Techicals
►Mechnical property for S460NL steel plate:
Thickness (mm) | ||||||||
S460NL | ≤ 16 | > 16 ≤ 40 | > 40 ≤ 63 | > 63 ≤ 80 | > 80 ≤ 100 | > 100 ≤ 150 | > 150 ≤ 200 | > 200 |
Yield strength (≥Mpa) | 460 | 440 | 430 | 410 | 400 | 380 | 370 | 370 |
≤ 100 | > 100 ≤ 200 | > 200 | ||||||
Tensile strength (Mpa) | 540-720 | 530-710 | 530-710 |
►Chemical composition for S460NL steel plate (Heat Analysis Max%)
Main chemical elements composition of S460NL steel plate | ||||||
C | Si | Mn | P | S | Nb | V |
0.20 | 0.60 | 1.00-1.70 | 0.025 | 0.020 | 0.05 | 0.20 |
Al(total) | Ti | Cr | Ni | Mo | Cu | N |
≥0.02 | 0.05 | 0.30 | 0.80 | 0.10 | 0.55 | 0.025 |