■ Overview
EN10025-3 S460N,S460N STEEL PLATE,S460N STEEL SHEET shall be rolled according to the below table of chemical composition.The limits applicable for the product analysis of structural steel plate s460n are given in the below table. The manufacturer shall inform the purchaser at the time of the enquiry and order which of the alloying elements appropriate to the steel grade required will be deliberately added to the material to be delivered. The product analysis shall be carried out when specified at the time of the order.Normalized heat treatment should be done for steel sheet S460N.
■ Full Data
Technical Requirements & Additional Services for S460N steel plate:
♦ Low temperature impacting test
♦ Rolling under standard NACE MR-0175 (HIC+SSCC)
♦ Ultrasonic test under EN 10160,ASTM A435,A577,A578
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
♦ Low temperature impacting test
♦ Rolling under standard NACE MR-0175 (HIC+SSCC)
♦ Ultrasonic test under EN 10160,ASTM A435,A577,A578
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
■ Techicals
►Mechnical property for S460N steel plate:
Thickness (mm) | ||||||||
S460N | ≤ 16 | > 16 ≤ 40 | > 40 ≤ 63 | > 63 ≤ 80 | > 80 ≤ 100 | > 100 ≤ 150 | > 150 ≤ 200 | > 200 |
Yield strength (≥Mpa) | 460 | 440 | 430 | 410 | 400 | 380 | 370 | 370 |
≤ 100 | > 100 ≤ 200 | > 200 | ||||||
Tensile strength (Mpa) | 540-720 | 530-710 | 530-710 |
►Chemical composition for S460N steel plate (Heat Analysis Max%)
Main chemical elements composition of S460N steel plate | ||||||
C | Si | Mn | P | S | Nb | V |
0.20 | 0.60 | 1.00-1.70 | 0.030 | 0.025 | 0.05 | 0.20 |
Al(total) | Ti | Cr | Ni | Mo | Cu | N |
≥0.02 | 0.05 | 0.30 | 0.80 | 0.10 | 0.55 | 0.025 |