■ Overview
Low temperature impacting test under -50 centigrade shall be done for structural S275NL,S275NL STEEL,S275NL steel plate.On longitudinal direction,the minimum values of impacting energy for S275NL test pieces shall be above 27 J,and on transverse direction,the minimum values of impacting energy for S275NL shall be above 16J according to steel standard EN 10025-3.Steel plate S275NL shall be supplied normalized or in an equivalent condition obtained by normalizing rolling.Xinsteel offer steel plate S275NL all over the world.
■ Full Data
Technical Requirements & Additional Services for S275NL steel plate:
♦ Low temperature impacting test
♦ Rolling under standard NACE MR-0175 (HIC+SSCC)
♦ Ultrasonic test under EN 10160,ASTM A435,A577,A578
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
♦ Low temperature impacting test
♦ Rolling under standard NACE MR-0175 (HIC+SSCC)
♦ Ultrasonic test under EN 10160,ASTM A435,A577,A578
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
■ Techicals
►Mechnical property for S275NL steel plate:
Thickness (mm) | ||||||||
S275NL | ≤ 16 | > 16 ≤ 40 | > 40 ≤ 63 | > 63 ≤ 80 | > 80 ≤ 100 | > 100 ≤ 150 | > 150 ≤ 200 | > 200 |
Yield strength (≥Mpa) | 275 | 265 | 255 | 245 | 235 | 225 | 215 | 205 |
≤ 100 | > 100 ≤ 200 | > 200 | ||||||
Tensile strength (Mpa) | 370-510 | 350-480 | 350-480 |
►Chemical composition for S275NL steel plate (Heat Analysis Max%)
Main chemical elements composition of S275NL steel plate | ||||||
C | Si | Mn | P | S | Nb | V |
0.16 | 0.40 | 0.50-1.50 | 0.025 | 0.020 | 0.05 | 0.05 |
Al(total) | Ti | Cr | Ni | Mo | Cu | N |
≥0.02 | 0.05 | 0.30 | 0.30 | 0.10 | 0.55 | 0.015 |