■ Overview
CCS Grade FH36,CCS FH36,CCS FH36 steel plate contains more Nickel and Nitrogen elements and less limited for Phosphorus and Sulphur in chemical composition.Nickel element can improve the weather resistance when sailing in ocean.Besides,CCS Grade FH36 shipbuilding steel plate have to be done low temperature impacting test under minus 60 centigree and done normalized heat treatment.
■ Full Data
Technical Requirements & Additional Services for CCS FH36 steel plate:
♦ High tension test
♦ Z-Test (Z15,Z25,Z35)
♦ Low temperature impacting test
♦ Ultrasonic test under ASTM A435,A577,A578
♦ Cetificated by ABS,LR,GL,BV,DNV,KR,NK,CCS,RINA
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
♦ High tension test
♦ Z-Test (Z15,Z25,Z35)
♦ Low temperature impacting test
♦ Ultrasonic test under ASTM A435,A577,A578
♦ Cetificated by ABS,LR,GL,BV,DNV,KR,NK,CCS,RINA
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
■ Techicals
►Mechnical property for CCS Grade FH36 shipbuilding structual steel:
Yield strength (≥Mpa) | Tensile strength (Mpa) | Elongation in ≥,% | |
355 | 490-620 | 200mm | 50mm |
19 | 22 |
►Chemical composition for CCS Grade FH36 ship steel (Heat Analysis Max%)
Main chemical elements composition of CCS Grade FH36 | ||||||
C | Si | Mn | P | S | Al (acid) min. | Nb |
0.16 | 0.50 | 0.90-1.60 | 0.025 | 0.025 | 0.015 | 0.02-0.05 |
V | Ti | Cu | Cr | Ni | Mo | N |
0.03-0.10 | 0.02 | 0.35 | 0.20 | 0.80 | 0.08 | 0.009 |