■ Overview
Normalized shipbuilding steel plate CCS Grade DH36 is a higher steel grade among shipbuilding steel.When rolling CCS Grade DH36,CCS DH36,CCS DH36 steel plate, TMCP or Normalized shall be done for heat treatment.Low temperature impacting test have to be done under minus 20 centigree for ship steel plate CCS Grade DH36.For improve the thickness-direct steel property for shipbuilding steel plate CCS Grade DH36,Z-test for CCS Grade DH36 is also necessary,our customers can choose three different classes,Z15,Z25 and Z35.
■ Full Data
Technical Requirements & Additional Services for CCS DH36 steel plate:
♦ High tension test
♦ Z-Test (Z15,Z25,Z35)
♦ Low temperature impacting test
♦ Ultrasonic test under ASTM A435,A577,A578
♦ Cetificated by ABS,LR,GL,BV,DNV,KR,NK,CCS,RINA
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
♦ High tension test
♦ Z-Test (Z15,Z25,Z35)
♦ Low temperature impacting test
♦ Ultrasonic test under ASTM A435,A577,A578
♦ Cetificated by ABS,LR,GL,BV,DNV,KR,NK,CCS,RINA
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
■ Techicals
►Mechnical property for CCS Grade DH36 shipbuilding structual steel:
Yield strength (≥Mpa) | Tensile strength (Mpa) | Elongation in ≥,% | |
355 | 490-620 | 200mm | 50mm |
19 | 22 |
►Chemical composition for CCS Grade DH36 ship steel (Heat Analysis Max%)
Main chemical elements composition of CCS Grade DH36 | ||||||
C | Si | Mn | P | S | Al (acid) min. | Nb |
0.18 | 0.10-0.50 | 0.90-1.60 | 0.035 | 0.035 | 0.015 | 0.02-0.05 |
V | Ti | Cu | Cr | Ni | Mo | |
0.05-0.10 | 0.02 | 0.35 | 0.20 | 0.40 | 0.08 |