■ Overview
CCS Grade AH40,CCS AH40,CCS AH40 steel plate is mainly used to building ships and vessels,so we also call this steel as CCS Grade AH40 ship plate,CCS Grade AH40 shipbuilding steel plate,CCS Grade AH40 marine steel plate or CCS Grade AH40 shipbuilding plate.Anyway these CCS Grade AH40 shipbuilding steel plates are the same and owned higher steel strength at minimum yield strength 390 Mpa and with minimum tensile strength 510 Mpa.Done low temperature impacting test for CCS Grade AH40 under zero centigree when rolling.
■ Full Data
Technical Requirements & Additional Services for CCS AH40 steel plate:
♦ High tension test
♦ Z-Test (Z15,Z25,Z35)
♦ Low temperature impacting test
♦ Ultrasonic test under ASTM A435,A577,A578
♦ Cetificated by ABS,LR,GL,BV,DNV,KR,NK,CCS,RINA
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
♦ High tension test
♦ Z-Test (Z15,Z25,Z35)
♦ Low temperature impacting test
♦ Ultrasonic test under ASTM A435,A577,A578
♦ Cetificated by ABS,LR,GL,BV,DNV,KR,NK,CCS,RINA
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
■ Techicals
►Mechnical property for CCS Grade AH40 shipbuilding structual steel:
Yield strength (≥Mpa) | Tensile strength (Mpa) | Elongation in ≥,% | |
390 | 510-650 | 200mm | 50mm |
19 | 22 |
►Chemical composition for CCS Grade AH40 ship steel (Heat Analysis Max%)
Main chemical elements composition of CCS Grade AH40 | ||||||
C | Si | Mn | P | S | Al (acid) min. | Nb |
0.18 | 0.10-0.50 | 0.90-1.60 | 0.035 | 0.035 | 0.015 | 0.02-0.05 |
V | Ti | Cu | Cr | Ni | Mo | |
0.05-0.10 | 0.02 | 0.35 | 0.20 | 0.40 | 0.08 |