■ Overview
Steel BV Grade AH36 is mainly used to building ships,so we also call this steel as BV Grade AH36 ship plate,BV Grade AH36 shipbuilding steel plate,BV Grade AH36 marine steel plate or BV Grade AH36 shipbuilding plate.Anyway these BV Grade AH36,BV AH36,BV AH36 steel plate are the same and owned higher steel strength at minimum yield strength 355 Mpa and with minimum tensile strength 490 Mpa.Done low temperature impacting test for BV Grade AH36 under zero centigree when rolling.
■ Full Data
Technical Requirements & Additional Services for BV AH36 steel plate:
♦ High tension test
♦ Z-Test (Z15,Z25,Z35)
♦ Low temperature impacting test
♦ Ultrasonic test under ASTM A435,A577,A578
♦ Cetificated by ABS,LR,GL,BV,DNV,KR,NK,CCS,RINA
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
♦ High tension test
♦ Z-Test (Z15,Z25,Z35)
♦ Low temperature impacting test
♦ Ultrasonic test under ASTM A435,A577,A578
♦ Cetificated by ABS,LR,GL,BV,DNV,KR,NK,CCS,RINA
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
■ Techicals
►Mechnical property for BV Grade AH36 shipbuilding structual steel:
Yield strength (≥Mpa) | Tensile strength (Mpa) | Elongation in ≥,% | |
355 | 490-620 | 200mm | 50mm |
19 | 22 |
►Chemical composition for BV Grade AH36 ship steel (Heat Analysis Max%)
Main chemical elements composition of BV Grade AH36 | ||||||
C | Si | Mn | P | S | Al (acid) min. | Nb |
0.18 | 0.10-0.50 | 0.90-1.60 | 0.035 | 0.035 | 0.015 | 0.02-0.05 |
V | Ti | Cu | Cr | Ni | Mo | |
0.05-0.10 | 0.02 | 0.35 | 0.20 | 0.40 | 0.08 |