■ Overview
Comparing common strength shipbuilding steel grades,BV Grade AH32,BV AH32,BV AH32 steel plate owned higher yield strength and tensile strength.Ship plate BV Grade AH32 is the Hull structural steel,with it's good toughness properties, higher strength,strong corrosion-resistance,the processing properties,and welding properties.In the steel standard ASTM A131/A131M,offshore steel grade ASTM A131 Grade AH32 is the best equvialent steel grade with BV Grade AH32.
■ Full Data
Technical Requirements & Additional Services for BV AH32 steel plate:
♦ High tension test
♦ Z-Test (Z15,Z25,Z35)
♦ Low temperature impacting test
♦ Ultrasonic test under ASTM A435,A577,A578
♦ Cetificated by ABS,LR,GL,BV,DNV,KR,NK,CCS,RINA
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
♦ High tension test
♦ Z-Test (Z15,Z25,Z35)
♦ Low temperature impacting test
♦ Ultrasonic test under ASTM A435,A577,A578
♦ Cetificated by ABS,LR,GL,BV,DNV,KR,NK,CCS,RINA
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
■ Techicals
►Mechnical property for BV Grade AH32 shipbuilding structual steel:
Yield strength (≥Mpa) | Tensile strength (Mpa) | Elongation in ≥,% | |
315 | 440-590 | 200mm | 50mm |
19 | 22 |
►Chemical composition for BV Grade AH32 ship steel (Heat Analysis Max%)
Main chemical elements composition of BV Grade AH32 | ||||||
C | Si | Mn | P | S | Al (acid) min. | Nb |
0.18 | 0.10-0.50 | 0.90-1.60 | 0.035 | 0.035 | 0.015 | 0.02-0.05 |
V | Ti | Cu | Cr | Ni | Mo | |
0.05-0.10 | 0.02 | 0.35 | 0.20 | 0.40 | 0.08 |