BS standard grade 275E steel plate with normalized heat treatment has good weldability and corrosion resistance in salt ocean water surroundings because of low sulphur and phosphorus contents.If need an even lower contains in P% and S%,BS grade 275EZ is better choice,the S% of 27EZ steel plate shall be equal or belows 0.008%.
■ Full Data
Technical Requirements & Additional Services for BS GR 275E steel plate:
♦ Z TEST (Z15,Z25,Z35) for through-thickness testing
♦ Charpy V-notch impacting test at -40 Degree centigrade
♦ Ultrasonic test under EN 10160,ASTM A435,A577,A578
♦ Simulated post-weld heat treatment
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
♦ Z TEST (Z15,Z25,Z35) for through-thickness testing
♦ Charpy V-notch impacting test at -40 Degree centigrade
♦ Ultrasonic test under EN 10160,ASTM A435,A577,A578
♦ Simulated post-weld heat treatment
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
■ Techicals
►Mechnical property for BS 275E steel plate:
Thickness (mm) | |||||||
BS Grade 275E | ≤ 16 | > 16 ≤ 40 | > 40 ≤ 63 | > 63 ≤ 100 | > 100 ≤ 120 | > 120 | |
Yield strength (≥Mpa) | 275 | 265 | |||||
≤ 100 | > 100 | ||||||
Tensile strength (Mpa) | 430-580 |
►Chemical composition for BS 275E steel plate (Ladle Analysis Max%)
Main chemical elements composition of BS grade 275E steel plate | ||||||||
C | Si | Mn | P | S | V | Nb+V | Nb | N |
0.16 | 0.10-0.50 | 1.50 | 0.040 | 0.030 | ||||
Cu | Alt | Cr | Mo | B | Ti | Ni | Cr+Mo+Ni+Cu | |