Quenched and tempered alloy steel plate A514 Grade S belongs to high yield and tensile strength steel plate.A514 Grade S,A514GrS,A514GrS steel plate furnished under ASTM A514/A514M shall conform to the requirements of the current edition of specification A6/A6M,for the ordered materials of steel A514 Gr.S. The manufacturer may reheat-treat plates that fail to meet the mechanical property requirements of this specification when rolling of high tension steel plate A514GrS.All mechanical property tests shall be repeated whenmaterial is resubmitted for inspection.
♦ High tension test
♦ Low temperature impacting test
♦ Simulated post-welded heat treatment (PWHT)
♦ Heat treatment under Quenching and Tempering
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
♦ Rolling under ASTM A6/A6M for Genenal requirements of structural used steel
►Mechnical property for A514GrS steel plate:
Thickness (mm) | Yield strength (≥Mpa) | Tensile strength (Mpa) | Elongation in ≥,% |
50mm | |||
T≤65 | 690 | 760-895 | 18 |
65<T | 620 | 690-895 | 16 |
►Chemical composition for A514GrS steel plate(Heat Analysis Max%)
Main chemical elements composition of A514GrS | ||||||||
C | Si | Mn | P | S | B | Mo | Nb | V |
0.11-0.21 | 0.15-0.45 | 1.10-1.50 | 0.035 | 0.020 | 0.001-0.005 | 0.10-0.60 | 0.06 | 0.06 |