Alloy structural A514 Grade M,A514GrM,A514GrM steel plate is under American steel standard ASTM A 514/A 514M.Alloy steel plate A514 Grade M,A514GrM contains more kinds alloy elements such as Nickel,Chromium,Molybdenum,Vanadium,Titanium,Zirconium,Copper and Boron when rolling.The chemical compostion of heat analysis shall be comply to the below table.As for the delivery condition,high strength steel plate ASTM A514 Grade M shall be under quenched and tempered.
♦ High tension test
♦ Low temperature impacting test
♦ Simulated post-welded heat treatment (PWHT)
♦ Heat treatment under Quenching and Tempering
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
♦ Rolling under ASTM A6/A6M for Genenal requirements of structural used steel
►Mechnical property for A514GrM steel plate:
Thickness (mm) | Yield strength (≥Mpa) | Tensile strength (Mpa) | Elongation in ≥,% |
50mm | |||
T≤65 | 690 | 760-895 | 18 |
65<T | 620 | 690-895 | 16 |
►Chemical composition for A514GrM steel plate (Heat Analysis Max%)
Main chemical elements composition of A514GrM steel plate | |||||||
C | Si | Mn | P | S | B | Mo | Ni |
0.12-0.21 | 0.20-0.35 | 0.45-0.70 | 0.035 | 0.035 | 0.001-0.005 | 0.45-0.60 | 1.20-1.50 |