■ Overview
A514 Grade H,A514GrH,A514GrH steel plate is a high strength steel material with the minimum yield strength at 690Mpa for the thickness belows 65mm,the tensile strength shall be within 760-895 Mpa. Quenched and tempered alloy steel plate A514 Grade H belongs to high yield and tensile strength steel plate.Rolling steel grade A514GrH furnished under ASTM A514/A514M shall conform to the requirements of the current edition of specification A6/A6M,for the ordered materials of steel A514 Gr.H,unless a conflict exists in which case this specification shall prevail.
■ Full Data
Technical Requirements & Additional Services for A514GrH steel plate:
♦ High tension test
♦ Low temperature impacting test
♦ Simulated post-welded heat treatment (PWHT)
♦ Heat treatment under Quenching and Tempering
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
♦ Rolling under ASTM A6/A6M for Genenal requirements of structural used steel
♦ High tension test
♦ Low temperature impacting test
♦ Simulated post-welded heat treatment (PWHT)
♦ Heat treatment under Quenching and Tempering
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
♦ Rolling under ASTM A6/A6M for Genenal requirements of structural used steel
■ Techicals
►Mechnical property for A514GrH steel plate:
Thickness (mm) | Yield strength (≥Mpa) | Tensile strength (Mpa) | Elongation in ≥,% |
50mm | |||
T≤65 | 690 | 760-895 | 18 |
65<T | 620 | 690-895 | 16 |
►Chemical composition for A514GrH steel plate (Heat Analysis Max%)
Main chemical elements composition of A514GrH steel plate | |||||||||
C | Si | Mn | P | S | B | Cr | Mo | Ni | V |
0.12-0.21 | 0.20-0.35 | 0.95-1.30 | 0.035 | 0.035 | 0.0005-0.005 | 0.40-0.65 | 0.20-0.30 | 0.30-0.70 | 0.03-0.08 |