■ Overview
A514 Grade C,A514GrC,A514GrC steel plate is under American steel standard ASTM A 514/A 514M specification.Till now Xinsteel can offer the maximum thickness for high strength steel plate A514Gr.C reaching to 300 millimeters with heat treatment of quenched and tempered.There are the similar steel grade as SA514 Grade C in steel standard ASME SA 514/SA 514M.When delivery steel materials ASTM A514Gr.C,steel mill would issued the original mill test certificate,also short as MTC which report the values of main chemical composition,mechanical property,all test result when rolling A514 Grade C steel plate.
■ Full Data
Technical Requirements & Additional Services for A514GrC steel plate:
♦ High tension test
♦ Low temperature impacting test
♦ Simulated post-welded heat treatment (PWHT)
♦ Heat treatment under Quenching and Tempering
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
♦ Rolling under ASTM A6/A6M for Genenal requirements of structural used steel
♦ High tension test
♦ Low temperature impacting test
♦ Simulated post-welded heat treatment (PWHT)
♦ Heat treatment under Quenching and Tempering
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
♦ Rolling under ASTM A6/A6M for Genenal requirements of structural used steel
■ Techicals
►Mechnical property for A514GrC steel plate:
Thickness (mm) | Yield strength (≥Mpa) | Tensile strength (Mpa) | Elongation in ≥,% |
50mm | |||
T≤65 | 690 | 760-895 | 18 |
65<T | 620 | 690-895 | 16 |
►Chemical composition for A514GrC steel plate (Heat Analysis Max%)
Main chemical elements composition of A514GrC steel plate | ||||||
C | Si | Mn | P | S | B | Mo |
0.10-0.20 | 0.15-0.30 | 1.10-1.50 | 0.035 | 0.035 | 0.001-0.005 | 0.15-0.30 |