■ Overview
A283 Grade D,A283GrD,A283GrD steel plate owned the minimum yield strength at 230 Mpa,and the tensile strength of mild steel plate A283GrD is within 415-550Mpa.When rolling A283 Grade D steel plate,Xinsteel would comply to steel standard A6/A6M and A283/A283M.For the thickness above 40mm of carbon steel plate A283 Grade D,Xinsteel suggest the end users to do Normalized heat treatment for these steel plates and improve the mechanical property.
■ Full Data
Technical Requirements & Additional Services for A283GrD steel plate:
♦ High tension test
♦ Low temperature impacting test
♦ Simulated post-welded heat treatment (PWHT)
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
♦ Rolling under ASTM A6/A6M for Genenal requirements of structural used steel
♦ High tension test
♦ Low temperature impacting test
♦ Simulated post-welded heat treatment (PWHT)
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
♦ Rolling under ASTM A6/A6M for Genenal requirements of structural used steel
■ Techicals
►Mechnical property for A283GrD steel plate:
Yield strength (≥Mpa) | Tensile strength (Mpa) | Elongation in ≥,% | |
230 | 415-550 | 200mm | 50mm |
20 | 23 |
►Chemical composition for A283GrD steel plate (Heat Analysis Max%)
Main chemical elements composition of A283GrD steel plate | ||||||
Thickness(mm) | C | Si | Mn | P | S | Cu (Min.) Cooper steel |
T≤40 | 0.27 | 0.40 | 0.90 | 0.035 | 0.04 | 0.20 |
40<T | 0.15-0.40 |