♦ Ultrasonic examination comply to A578/A578M A577/A577M A435/A435M
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ PMI test report,Cutting and welding as per end user’s demands
♦ Packing with water-resistance paper and Non-fumigation wooden crates
♦ Definiations for Mechanical testing comply to A370
♦ Practices for detecting susceptibility to Intergranular corrosion in Austenitic stainless steels
♦ PMI test report,Cutting and welding as per end user’s demands
►Mechnical property for Stainless steel plate SUS347
Stainless steel sheet A240 TP347 |
||||
Yield strength (≥Mpa) |
Tensile strength (≥Mpa) |
Elogation in 50mm min. % |
Hardness, Max |
|
Brinell HBW |
Rockwell HRBW |
|||
205 |
515 |
40 |
201 |
92 |
►Chemical composition for Stainless steel plate SUS347 (Heat Analysis Max%)
Main chemical elements composition of Stainless steel sheet A240 TP347 |
|||||
C |
Mn |
P |
S |
Si |
Cr |
0.08 |
2.00 |
0.045 |
0.030 |
0.75 |
17.0-19.0 |
Ni |
Mo |
N |
Cb |
Al |
Ti |
9.0-13.0 |
- |
- |
8*C-1.0 |
- |
- |