  • Thickness: 0.3mm-100mm
  • Width: 200mm-4000mm
  • Length: 1000mm-18000mm
  • Heat Treatment: Pickling,Solid Solution,Annealing
  • Steel Standard: ASTM A240/A240M ASTM A480/A480M ASME SA240 / SA240,ASME SA480 /SA480M
  • Surface Condition: No.1,No.2B,No.2D,Bright Annealed Finish,Polish Finish,Satin Finish,High Luster Finish,Mirror Finish
(※ Click this button to inquiry)
■ Overview
HOT ROLLED STAINLESS PLATE A240 2507 has excellent resistance to spot corrosion, crevice corrosion and uniform corrosion due to the high content of chromium and molybdenum in chemical composition.Stainless steel plate A240 2507 is used in oil and gas industry,Offshore oil platform,water treatment and water supply system,Petrochemical equipment,fire fighting system,spray system and water stabilization system.
■ Full Data
Technical Requirements & Additional Services for Stainless steel sheet A240 2507:
♦  Ultrasonic examination comply to A578/A578M A577/A577M A435/A435M
♦  Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2 
♦  PMI test report,Cutting and welding as per end user’s demands 
♦  Grain sizes test according to ASTM E112
♦  Definiations for Mechanical testing comply to A370
♦  Packing with water-resistance paper and Non-fumigation wooden crates
■ Techicals

►Mechnical property for Stainless steel plate A240 2507

HOT ROLLED STAINLESS PLATE A240 2507

Yield strength (≥Mpa)

Tensile strength (≥Mpa)

Elogation in 50mm min. %

Hardness, Max

Brinell

HBW

Rockwell

HRBW

550

795

15

310

32


►Chemical composition for Stainless steel plate A240 2507 (Heat Analysis Max%)

Main chemical elements composition of HOT ROLLED STAINLESS PLATE A240 2507

C

Mn

P

S

Si

Cr

0.03

1.2

0.035

0.020

0.8

24-26

Ni

Mo

N

Cu

Al

Ti

6.0-8.0

3.0-5.0

0.24-0.32

0.50

-

-

 

 