■ Overview
A203 Grade B,A203GrB steel plate,A203GrB steel sheet with minimum yield strength at 275 Mpa,higher than A203 Grade A pressure vessel steel plate at 255 Mpa,and tensile strength shall be above 480 Mpa for steel plate SA203 Grade B.Ultrasonic examination for pressure vessel steel plate A203 Grade B,there are A 435/A 435M,A 577/A 577M,A 578/A 578M and A578/A578M including three levels,A578-A,A578-B,A578-C.
■ Full Data
Technical Requirements & Additional Services for A203GRB steel plate:
♦ High tension test
♦ Low temperature impacting test
♦ Simulated post-welded heat treatment (PWHT)
♦ Rolling under standard NACE MR-0175 (HIC+SSCC)
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
♦ High tension test
♦ Low temperature impacting test
♦ Simulated post-welded heat treatment (PWHT)
♦ Rolling under standard NACE MR-0175 (HIC+SSCC)
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
■ Techicals
► Mechnical property for A203 Grade B steel plate:
►Chemical composition for A203 Grade B steel plate (Heat Analysis Max%)
Yield strength (≥Mpa) | Tensile strength (Mpa) | Elongation in ≥,% | |
275 | 485-620 | 200mm | 50mm |
17 | 21 |
►Chemical composition for A203 Grade B steel plate (Heat Analysis Max%)
Main chemical elements composition of A203 Grade B steel plate | ||||||
Thickness(mm) | C | Si | Mn | P | S | Ni |
T≤50 | 0.21 | 0.15-0.40 | 0.70 | 0.035 | 0.035 | 2.10-2.50 |
50<T | 0.24 | 0.80 |