■ Overview
The similar shipbuilding steel grade A131 Grade EH40,A131GrEH40 steel plate,A131GrEH40 steel sheet in steel stand ASTM A131/A131M is mainly used on offshore and oil platform project. Actually A131 Grade EH40 owned the same chemical composition and mechnical property as ABS Grade EH40 shipbuilding steel plates.These two steel grades are in our rolling catalogs.
■ Full Data
Technical Requirements & Additional Services for A131GrEH40 steel plate:
♦ High tension test
♦ Z-Test (Z15,Z25,Z35)
♦ Low temperature impacting test
♦ Ultrasonic test under ASTM A435,A577,A578
♦ Cetificated by ABS,LR,GL,BV,DNV,KR,NK,CCS,RINA
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
♦ High tension test
♦ Z-Test (Z15,Z25,Z35)
♦ Low temperature impacting test
♦ Ultrasonic test under ASTM A435,A577,A578
♦ Cetificated by ABS,LR,GL,BV,DNV,KR,NK,CCS,RINA
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
■ Techicals
►Mechnical property for A131GrEH40 steel plate:
Yield strength (≥Mpa) | Tensile strength (Mpa) | Elongation in ≥,% | |
390 | 510-650 | 200mm | 50mm |
19 | 22 |
►Chemical composition for A131GrEH40 steel plate (Heat Analysis Max%)
Main chemical elements composition of A131GrEH40 steel plate | ||||||
C | Si | Mn | P | S | Al (acid) min. | Nb |
0.18 | 0.10-0.50 | 0.90-1.60 | 0.035 | 0.035 | 0.015 | 0.02-0.05 |
V | Ti | Cu | Cr | Ni | Mo | |
0.05-0.10 | 0.02 | 0.35 | 0.20 | 0.40 | 0.08 |