■ Overview
Shipyards use shipbuilding A131 Grade AH36,A131GrAH36 steel plate,A131GrAH36 steel sheet to construct tanks and vessels in ships cause A131 Grade AH36 ship plate owned the higher yield strength and tensile strength.Xinsteel group owned tens of stock warehouses in port cities in China,there are thousands tons of shipbuilding steel plate and sheet and angles and buld flats in stock which are ready to ship on board.Different thicknesses,width mainly in 2000-2500mm,length mainly in 6000-12000mm for A131 Grade AH36 steel plate
■ Full Data
Technical Requirements & Additional Services for A131GrAH36 steel plate:
♦ High tension test
♦ Z-Test (Z15,Z25,Z35)
♦ Low temperature impacting test
♦ Ultrasonic test under ASTM A435,A577,A578
♦ Cetificated by ABS,LR,GL,BV,DNV,KR,NK,CCS,RINA
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
♦ High tension test
♦ Z-Test (Z15,Z25,Z35)
♦ Low temperature impacting test
♦ Ultrasonic test under ASTM A435,A577,A578
♦ Cetificated by ABS,LR,GL,BV,DNV,KR,NK,CCS,RINA
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
■ Techicals
►Mechnical property for A131GrAH36 steel plate:
Yield strength (≥Mpa) | Tensile strength (Mpa) | Elongation in ≥,% | |
355 | 490-620 | 200mm | 50mm |
19 | 22 |
►Chemical composition for A131GrAH36 steel plate (Heat Analysis Max%)
Main chemical elements composition of A131GrAH36 steel plate | ||||||
C | Si | Mn | P | S | Al (acid) min. | Nb |
0.18 | 0.10-0.50 | 0.90-1.60 | 0.035 | 0.035 | 0.015 | 0.02-0.05 |
V | Ti | Cu | Cr | Ni | Mo | |
0.05-0.10 | 0.02 | 0.35 | 0.20 | 0.40 | 0.08 |