♦ Ultrasonic examination comply to A578/A578M A577/A577M A435/A435M
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ PMI test report,Cutting and welding as per end user’s demands
♦ Packing with water-resistance paper and Non-fumigation wooden crates
►Mechnical property for Stainless steel sheet SA240 334
Stainless steel plate SA240 334 |
||||
Yield strength (≥Mpa) |
Tensile strength (≥Mpa) |
Elogation in 50mm min. % |
Hardness, Max |
|
Brinell HBW |
Rockwell HRBW |
|||
205 |
515 |
40 |
217 |
95 |
►Chemical composition for Stainless steel sheet SA240 334 (Heat Analysis Max%)
Main chemical elements composition of Stainless steel plate SA240 334 |
|||||
C |
Mn |
P |
S |
Si |
Cr |
0.08 |
1.00 |
0.030 |
0.015 |
1.00 |
18.0-20.0 |
Ni |
Mo |
N |
Cb |
Al |
Ti |
19.0-21.0 |
- |
- |
- |
0.15-0.60 |
0.15-0.60 |