►Mechnical property for S32550 Stainless steel plate
SA240 255 stainless plate |
||||
Yield strength (≥Mpa) |
Tensile strength (≥Mpa) |
Elogation in 50mm min. % |
Hardness, Max |
|
Brinell HBW |
Rockwell HRBW |
|||
550 |
760 |
15 |
302 |
32 |
►Chemical composition for S32550 Stainless steel plate (Heat Analysis Max%)
Main chemical elements composition of SA240 255 stainless plate |
|||||
C |
Mn |
P |
S |
Si |
Cr |
0.04 |
1.5 |
0.040 |
0.030 |
1.00 |
24-27 |
Ni |
Mo |
N |
Cu |
Al |
Ti |
4.5-6.5 |
2.9-3.9 |
0.10-0.25 |
1.5-2.5 |
- |
- |