♦ Ultrasonic examination comply to SA578/SA578M SA577/SA577M SA435/SA435M
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ PMI test report,Cutting and welding as per end user’s demands
♦ Packing with water-resistance paper and Non-fumigation wooden crates
►Mechnical property for Stainless steel sheet SA240 305
UNS S30500 Stainless plate |
||||
Yield strength (≥Mpa) |
Tensile strength (≥Mpa) |
Elogation in 50mm min. % |
Hardness, Max |
|
Brinell HBW |
Rockwell HRBW |
|||
170 |
485 |
40 |
183 |
88 |
►Chemical composition for Stainless steel sheet SA240 305 (Heat Analysis Max%)
Main chemical elements composition of UNS S30500 Stainless plate |
|||||
C |
Mn |
P |
S |
Si |
Cr |
0.12 |
2.00 |
0.045 |
0.030 |
0.75 |
17.0-19.0 |
Ni |
N |
Cu |
Mo |
Al |
Ti |
10.5-13.0 |
- |
- |
- |
- |
- |