Quenching and Tempering heat treatment shall be done for ASME SA203 Grade F steel plate when supplying.The minimum thickness can reach till 5 millimeter for rolling SA203GRF steel sheet from Xinsteel.Non-destructive inspection shall be done for SA203 Grade F steel plate according to ASME SA578 Level A,Level B or C.
■ Full Data
Technical Requirements & Additional Services for SA203 Grade F steel plate:
♦ Charpy V-nocth impacting test
♦ Simulated post-welded heat treatment (PWHT)
♦ Rolling under standard NACE MR-0175 (HIC+SSCC)
♦ Shot blasting comply to SA2.5 and Painting with shop primer
♦ Quenched and Tempered heat treatment for steel plate
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.2 with third party insepction witness
♦ Cutting,Welding,Rough Machining,Finish Maching,Drilling,Milling,Grinding according to CAD Drawing
♦ Charpy V-nocth impacting test
♦ Simulated post-welded heat treatment (PWHT)
♦ Rolling under standard NACE MR-0175 (HIC+SSCC)
♦ Shot blasting comply to SA2.5 and Painting with shop primer
♦ Quenched and Tempered heat treatment for steel plate
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.2 with third party insepction witness
♦ Cutting,Welding,Rough Machining,Finish Maching,Drilling,Milling,Grinding according to CAD Drawing
■ Techicals
►Mechnical property for SA203 Grade F steel plate:
Thickness(mm) | Yield strength (≥Mpa) | Tensile strength (Mpa) | Elongation in ≥,% | |
200mm | 50mm | |||
T≤50 | 380 | 550-690 | ... | 20 |
50<T | 345 | 515-655 |
►Chemical composition for SA203 Grade F steel plate (Heat Analysis Max%)
Main chemical elements composition of SA203 Grade F | ||||||
Thickness(mm) | C | Si | Mn | P | S | Ni |
T≤50 | 0.20 | 0.15-0.40 | 0.70 | 0.035 | 0.035 | 3.25-3.75 |
50<T | 0.25 | 0.80 |